Brand Name : Lonroy
Model Number : LRC
Certification : Includes Calibration Certification
Place of Origin : China
MOQ : 1
Price : Negotaible
Payment Terms : L/C,D/A,D/P,T/T,Western Union
Supply Ability : 200
Delivery Time : 5-8 work days
Packaging Details : Wooden package
Power Supply : 380V AC, 3 kW
Sample Dimensions : Ø50 × 50 mm
Sample Load Pressure : 0.2 MPa
Max. Heating Temperature : 1650°C
Warranty : 1 Year
This instrument is used to test the resistance of refractory materials under high-temperature and load softening conditions, which is an important indicator for evaluating the high-temperature mechanical properties of refractory materials. It complies with the national standards GB/T5073-2005 "Test Method for Creep of Refractory Materials under Pressure" and GB/T5989-2008 "Test Method for Softening Temperature under Load of Refractory Materials". It is equipped with a computer for automatic testing and data processing, automatically generating and saving the temperature and deformation curve graphs.
2.Configuration:
Includes 1 LRC testing instrument main unit, 1 testing software, 1 set of communication interface and data cable, 1 high-temperature test column, 1 high-temperature test column, 1 B-type thermocouple, 1 set of silicon molybdenum rods, 1 set of weights, and 1 desktop computer (configured according to the contract).
3.Technical Parameter
| Parameter | Specification |
| Max. Heating Temperature | 1650°C |
| Temperature Control | Programmable Microcomputer Control Accuracy: ±1°C |
| Deformation Measurement Error | ≤ 0.01 mm |
| Sample Dimensions | Ø50 × 50 mm |
| Sample Load Pressure | 0.2 MPa |
| Power Supply | 380V AC, 3 kW |
| Heating Elements | Molybdenum Disilicide (MoSi2) Elements |
|
|