| Sign In | Join Free | My lightneasy.org |
|
Type : Testing Machine
Accuracy : ---
Brand Name : LONROY
Place of Origin : Guangdong, China
Application : Laboratory Testing
customized support : OEM, ODM, OBM, Software Reengineering
power : ---
Protection Class : IP57
Voltage : 220 V, 380 V
warranty : 1 Year
MOQ : 1
Price : $6,830
DSC Differential Scanning Calorimeter Calorimetry Thermal Analysis Machine Analyzer/DSC Differential Calorimeter Analyzer

Product Introduction:
LR-dsc300c is the company launched DSC series of products with the highest accuracy of one, the sensor is the use of imported material E-couple, high precision, high sensitivity, good repeatability, signal acquisition circuit shielding protection, strong anti-interference, baseline stability and repeatability is very high.
Dz-dsc300 differential scanning calorimeter, can be glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature and product stability, oxidation induction period and other tests.It is qualified for the research of pipe, polymer, chemical, food, medical and other fields, and serves universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.
DSC Differential Scanning Calorimeter Calorimetry Thermal Analysis Machine Analyzer/DSC Differential Calorimeter Analyzer
Technical parameters:
|
Temperature Range |
-40~600℃ |
|
Temperature Resolution |
0.001℃ |
|
Temperature Fluctuation |
±0.001℃ |
|
Temperature Repeatability |
±0.01℃ |
|
Heating Rate |
0.1~80℃/min |
|
Constant Temperature Time |
Program setting ≤24h |
|
Temperature Control Mode |
Heating, constant temperature, cooling (automatic program control) |
|
DSC Range |
0~±600mW |
|
DSC Resolution |
0.01μW |
|
DSC Sensitivity |
0.001mW |
|
Power Supply |
AC220V/50Hz or customized |
|
Atmosphere Control Gas |
Nitrogen, oxygen (program setting/automatic switch) |
|
Gas Flow Rate |
0-300ml/min |
|
Gas Pressure |
0.2MPa |
|
Display Mode |
24-bit color, 7-inch LCD touch screen display |
|
Data Interface |
Standard USB interface |
|
Parameter Calibration |
Equipped with standard materials (indium, tin); users can adjust temperature independently |
|
The instrument has multiple groups of thermocouples, one group to measure sample temperature, one group to measure furnace body temperature, and one group to measure internal environment temperature |
|
|
Cooling Device |
Semiconductor cooling device (optional liquid nitrogen refrigeration & lt;-150~550℃& gt;) |
Technical features:
1. Industrial grade 7 inch touch screen, display rich information
2. New furnace body structure, better baseline, higher accuracy.Heating adopts indirect conduction mode, high uniformity and stability, reduce pulse radiation, better than the traditional heating mode.
3.USB communication interface, strong commonality, reliable communication without interruption, support self-recovery connection function.
4. Automatic switching of two air flow, fast switching speed, short stability time.At the same time, a protective gas input is added.
5. Software is simple and easy to operate.
6. Ultra-high sensitivity, accuracy, 0.001 MW, 0.001℃
7. Exquisite technical indicators, superior performance, cost-effective, widely used

Furnace body structure
Test map: glass transition temperature

Test map: melting point and enthalpy

|
|
DSC Differential Scanning Calorimeter Calorimetry Thermal Analysis Machine Analyzer/DSC Differential Calorimeter DSC Images |